Hey Everyone,
Got my new Heddman Hedders for my 79 k20 and was in the process of stripping the protective paint so I could paint them with a ceramic and I found something I wasnt expecting. Looks like one of the spots that they had it clamped during fabrication. It goes almost all the way around it and one part isnt too deep and within what I would expect but the other bigger one looks like its at least halfway through the pipe. Its deep enough to make a glare from my camera flash...
I was planning on returning them but someone in my build thread said that it was normal. Im not convinced lol. It seems like poor craftsmanship to me and a weak point in the tubes that will get hotter than the rest because it cant dissipate the heat as quickly. Which would lead to the metal in that spot becoming brittle.
Jeggs wasn't super helpful with the return either and was thinking about calling Heddman but I don't know if they handle something like this or if I should go through Jeggs. I have to wait over a week to get my new headers if I do return them. And no consolation prize for my troubles
Just don't want to wait a week or two to get them back and then my next set with all the protective paint still on, have the same thing. I spent like 4 hours on those already with some really nasty chemicals that I don't like using. Also don't want to be a jerk and make a bunch of underpaid people work extra at Jeggs and Hedman for no reason. Let me know what you think, thanks.
Got my new Heddman Hedders for my 79 k20 and was in the process of stripping the protective paint so I could paint them with a ceramic and I found something I wasnt expecting. Looks like one of the spots that they had it clamped during fabrication. It goes almost all the way around it and one part isnt too deep and within what I would expect but the other bigger one looks like its at least halfway through the pipe. Its deep enough to make a glare from my camera flash...
I was planning on returning them but someone in my build thread said that it was normal. Im not convinced lol. It seems like poor craftsmanship to me and a weak point in the tubes that will get hotter than the rest because it cant dissipate the heat as quickly. Which would lead to the metal in that spot becoming brittle.
Jeggs wasn't super helpful with the return either and was thinking about calling Heddman but I don't know if they handle something like this or if I should go through Jeggs. I have to wait over a week to get my new headers if I do return them. And no consolation prize for my troubles
Just don't want to wait a week or two to get them back and then my next set with all the protective paint still on, have the same thing. I spent like 4 hours on those already with some really nasty chemicals that I don't like using. Also don't want to be a jerk and make a bunch of underpaid people work extra at Jeggs and Hedman for no reason. Let me know what you think, thanks.